您要查找的是不是:
- This provides the importance basis for protecting from erroneous judgement in macroetching test of forgings. 为锻件低倍试验中防止误判提供重要依据。
- The star cracks in macrostructure appear in some hypo-peritectic continuous cast alloy blooms and these cracks cannot be stock completely by hot rolling reduction ratio, macroetching testing and SEM. 摘要一些亚包晶合金钢连铸大方坯出现低倍星状裂纹,在一定的压缩比下经轧制仍不能完全消除这种低倍缺陷。
- The star cracks in macrostructure appear in some hypo-peritectic continuous cast alloy blooms and these cracks cannot be stuck completely by hot rolling reduction ratio,macroetching testing and SEM. 一些亚包晶合金钢连铸大方坯出现低倍星状裂纹,在一定的压缩比下经轧制仍不能完全消除这种低倍缺陷。
- Standard Method of Macroetch Testing Steel Bars, Billets, Blooms, and Forgings 由棒材,坯段,大方坯和锻件组成的钢制品的宏观浸蚀试验,检验及评定
- macroetch vt. 宏观腐蚀
- macroetching 宏观腐蚀,粗形浸蚀,宏观组织腐蚀,深度浸蚀,宏观浸蚀