Inner-tailpipe nozzle, which cast by investment casting with superalloy K487, is one of the key components of the spaceflight engine.
英
美
释义
内涵尾喷管是某航天发动机的关键部件,采用可焊接铸造高温合金K487无余量整体精密铸造而成。