In transient crack zone, the SEM fractographs of base metal consisted of equal-axis ductile voids, the fusion zone was mainly consisted of course transgranular cleavage facets.
英
美
释义
在瞬断区,母材由等轴韧窝组成,而熔合区主要为粗大的穿晶解理平面。