An investigation was undertaken to assess the quality of P/M superalloy EP741NP disk.The chemical and phase analysis as well as mechanical property test were performed.
英
美
释义
摘要对EP741NP合金盘坯进行了化学成分和相分析、力学性能测试、组织和断口形貌观察,并做了热处理试验。